The upper limit of catalyst performance is often determined by the purity of the support raw materials. Many people focus on the main content of magnesium oxide while overlooking three hidden indicators—chlorides, sulfates, and loss on ignition (LOI)—which are precisely what determine whether a catalyst can stably achieve industrial implementation.

The risks posed by chlorides carry the dual attributes of catalyst poisoning and equipment corrosion. In high-temperature systems such as sulfur-tolerant shift and hydrogenation, chloride ions induce the migration and agglomeration of active metals, leading to a decline in the number of active sites. Accompanied by water vapor, they generate acidic media that continuously corrode reaction equipment, creating safety hazards. In many catalytic projects, the main content meets standards while chloride levels exceed the limit; small-scale trials pass, yet stability collapses upon scale-up production—this is a common pain point in the industry.
Sulfate residues alter the surface chemical environment of the support. Sulfate ions adsorb onto the surface of magnesium oxide, introducing unnecessary acid sites and inducing side reactions. Under sustained high temperatures, they slowly decompose and generate gas, causing the support skeleton to become loose and its compressive strength to drop. For industrial catalysts requiring long-term cyclic operation, once the support structure is damaged, the overall service life will be drastically shortened.
Loss on ignition directly reflects the calcination degree of the magnesium oxide precursor. An excessively high LOI indicates that the raw material contains relatively high amounts of magnesium hydroxide, magnesium carbonate, and adsorbed moisture. During the catalyst calcination heating process, the continuous release of gases easily causes blistering and cracking of the support, leading to pore volume and pore size deviating from design values. The released water vapor also causes the loss of active components, resulting in pronounced performance fluctuations between different batches.
Messi Biology customizes magnesium oxide specifically for catalytic scenarios, adopting a targeted purification process to strictly control chloride and sulfate residues and stabilize loss on ignition. This ensures that the pore structure and active adsorption sites of each batch of support remain consistent, adapting to multiple catalytic routes such as sulfur-tolerant shift, desulfurization, and hydrogen production.
Industrial catalysis pursues continuous stability, and raw material impurity control cannot wait until finished product testing for remediation. Selecting magnesium oxide with low chloride, low sulfate, and stable loss on ignition from the source is a reliable means to control finished catalyst consistency, extend service cycles, and reduce unit failures, while also serving as the foundation for achieving stable mass production of catalytic materials.